GA-9540 na ɛwɔ hɔ.
Herchy .
| a ɛwɔ hɔ no ho adanse: | |
|---|---|
| Dodow: | |
Sɔhwɛ: Aduru a wɔde sa yareɛ no mu 1% (50% a wɔde DBPMH ahyɛ mu wɔ silicone gum mu), 175°C x 5min x 15MPa.
| Product parameters . | ||||
| Adwadeɛ | GA-9540 na ɛwɔ hɔ. |
GA-9550 na ɛwɔ hɔ | GA-9560 na ɛwɔ hɔ. | GA-9570 na ɛwɔ hɔ. |
| Mmaeɛ | Translucent . | |||
| William plastic a ɛwɔ hɔ no . |
155 |
200 |
220 |
250 |
| Hardness (Shorea) . |
40 |
50 |
60 |
70 |
| density(g/cm3) . | 1.14 |
1.17 |
1.19 |
1.20 |
| Ahoɔden a ɛyɛ den (MPa) . |
8.0 |
9.0 |
10.0 |
11.0 |
| Elongation(%) . | 600 |
500 |
450 |
300 |
| Ahoɔden a ɛtetew (kn/m) . | 14 |
25 |
25 |
25 |