GA-9540
Herchy
| Boteng ba FDA: | |
|---|---|
| Bongata: | |
Teko: 1% ea moemeli oa phekolo (50% pente ea DBPMH ka silicone gum), 175 ° C x 5min x 15MPa.
| Lihlahisoa tsa lihlahisoa | ||||
| Sehlahisoa | GA-9540 |
GA-9550 | GA-9560 | GA-9570 |
| Ponahalo | Translucent | |||
| William polasetiki |
155 |
200 |
220 |
250 |
| Ho thatafala (LebopoA) |
40 |
50 |
60 |
70 |
| Boima ba 'mele(g/cm3) | 1.14 |
1.17 |
1.19 |
1.20 |
| Tensile Matla (MPa) |
8.0 |
9.0 |
10.0 |
11.0 |
| Elongation(%) | 600 |
500 |
450 |
300 |
| Matla a ho lla (kN/m) | 14 |
25 |
25 |
25 |