GA-9540
Herchy
| Availability: | |
|---|---|
| Rahi: | |
Whakamatau: 1% o te kaihoko whakaora (50% te whakapiri o te DBPMH i roto i te kapia silicone), 175°C x 5min x 15MPa.
| Tawhā hua | ||||
| Hua | GA-9540 |
GA-9550 | GA-9560 | GA-9570 |
| Te ahua | Puatarangi | |||
| Wiremu kirihou |
155 |
200 |
220 |
250 |
| Maama (ShoreA) |
40 |
50 |
60 |
70 |
| Kiato(g/cm3) | 1.14 |
1.17 |
1.19 |
1.20 |
| Te kaha o te kaha (MPa) |
8.0 |
9.0 |
10.0 |
11.0 |
| Whakaroa(%) | 600 |
500 |
450 |
300 |
| Te kaha roimata (kN/m) | 14 |
25 |
25 |
25 |