GA-9540
Herchy
| Disponibilite: | |
|---|---|
| Kantite: | |
Tès: 1% nan ajan geri (50% keratin nan DBPMH nan jansiv silikon), 175 °C x 5min x 15MPa.
| Paramèt pwodwi | ||||
| Pwodwi | GA-9540 |
GA-9550 | GA-9560 | GA-9570 |
| Aparans | Translusid | |||
| William plastisit |
155 |
200 |
220 |
250 |
| Dite (ShoreA) |
40 |
50 |
60 |
70 |
| Dansite (g/cm3) | 1.14 |
1.17 |
1.19 |
1.20 |
| Fòs rupture (MPa) |
8.0 |
9.0 |
10.0 |
11.0 |
| elongasyon (%) | 600 |
500 |
450 |
300 |
| Fòs chire (kN/m) | 14 |
25 |
25 |
25 |