GA-9540
Herchy
| Availability: | |
|---|---|
| habetsahana: | |
Fitsapana: 1% amin'ny fanafody manasitrana (50% pasteur DBPMH amin'ny silikôla silikônina), 175 ° C x 5min x 15MPa.
| Masontsivana vokatra | ||||
| vokatra | GA-9540 |
GA-9550 | GA-9560 | GA-9570 |
| Bika Aman 'endrika | Translucent | |||
| William plasticity |
155 |
200 |
220 |
250 |
| Hardness (ShoreA) |
40 |
50 |
60 |
70 |
| Hateza (g/cm3) | 1.14 |
1.17 |
1.19 |
1.20 |
| Henjana (MPa) |
8.0 |
9.0 |
10.0 |
11.0 |
| Elongation(%) | 600 |
500 |
450 |
300 |
| Herin-dranomaso (kN/m) | 14 |
25 |
25 |
25 |