GA-71××
Herchy
| Availability: | |
|---|---|
| Quantity: | |
Test: 1% of curing agent (50% paste of DBPMH ins小conegum), 175° x 5min x 15MPa.
| Product parameters | ||||||
| Product | GA-7120 |
GA-7130 | GA-7131 | GA-7151 | GA-7161 | GA-7171 |
| Appearance | Translucent | |||||
| Williamplasticity |
140 |
160 |
200 |
220 |
240 |
280 |
| Hardness (ShoreA) |
25 |
30 |
40 |
50 |
60 |
70 |
| Density(g/cm3) | 1.10 |
1.12 |
1.14 |
1.18 |
1.20 |
1.23 |
| Tensilestrength (MPa) |
7 |
8 |
8 |
8 |
8 |
7 |
| Elongation(%) | 800 |
850 |
750 |
650 |
500 |
400 |
| Tearstrength (kN/m) | 14 |
20 |
30 |
30 |
22 |
22 |