GA-71××
Herchy
| Argaeledd: | |
|---|---|
| Nifer: | |
Prawf: 1% o asiant halltu (50% past o DBPMH ins小conegum), 175 ° x 5 munud x 15MPa.
| Paramedrau cynnyrch | ||||||
| Cynnyrch | GA- 7120 |
GA- 7130 | GA-7131 | GA- 7151 | GA- 7161 | GA- 7171 |
| Ymddangosiad | Tryleu | |||||
| Williamplastigedd |
140 |
160 |
200 |
220 |
240 |
280 |
| Caledwch (ShoreA) |
25 |
30 |
40 |
50 |
60 |
70 |
| Dwysedd(g/cm3) | 1.10 |
1.12 |
1.14 |
1.18 |
1.20 |
1.23 |
| Cryfder tynnol (MPa) |
7 |
8 |
8 |
8 |
8 |
7 |
| elongation(%) | 800 |
850 |
750 |
650 |
500 |
400 |
| Cryfder dagrau (kN/m) | 14 |
20 |
30 |
30 |
22 |
22 |