GA-71×× na ɛwɔ hɔ
Herchy a ɔyɛ ɔbarima
| Nea Ɛwɔ Hɔ: | |
|---|---|
| Dodow: | |
Sɔhwɛ: 1% a ɛyɛ aduru a wɔde sa yare (50% a wɔde ahyɛ DBPMH ins小conegum mu), 175° x 5min x 15MPa.
| Nneɛma a wɔyɛ no parameters | ||||||
| Adwadeɛ | GA-7120 na ɛwɔ hɔ |
GA-7130 na ɛwɔ hɔ | GA-7131 na ɛwɔ hɔ | GA-7151 na ɛwɔ hɔ | GA-7161 na ɛwɔ hɔ | GA-7171 na ɛwɔ hɔ |
| Mmaeɛ | Ɛyɛ nea ɛyɛ translucent | |||||
| Williamplasticity a wɔde yɛ nneɛma |
140 |
160 |
200 |
220 |
240 |
280 |
| Nneɛma a ɛyɛ den (ShoreA) . |
25 |
30 |
40 |
50 |
60 |
70 |
| Nsuo a ɛyɛ den(g/cm3) . | 1.10 |
1.12 |
1.14 |
1.18 |
1.20 |
1.23 |
| Ahoɔden a ɛtwetwe ade (MPa) . |
7 |
8 |
8 |
8 |
8 |
7 |
| Ntrɛwmu(%) . | 800 |
850 |
750 |
650 |
500 |
400 |
| Nusu ahoɔden (kN/m) . | 14 |
20 |
30 |
30 |
22 |
22 |