GA-71×× Silicone Rubber for Molding with High Tear ƙarfi (HCR)

Aikace-aikace: kowane nau'i na kwasfa, walat, agogo, bandeji na roba, kayan ado da sauran samfuran ƙarfi.
Maɓalli masu mahimmanci: babban tashin hankali, kyawawan kaddarorin saki, kyakkyawan tsari, wuce amincin RoHS, REACH, da FDA.
  • GA-71××

  • Herchy

samuwa:
Yawan:

Gwaji: 1% na wakili mai warkewa (manna 50% na DBPMH ins小conegum), 175° x 5min x 15MPa.


Siffofin samfur
Samfura GA-7120
GA-7130 GA-7131 GA-7151 GA-7161 GA-7171
Bayyanar Translucent
Williamplasticity
140
160
200
220
240
280
Hardness (ShoreA)
25
30
40
50
60
70
Girma (g/cm3) 1.10
1.12
1.14
1.18
1.20
1.23
Ƙarfin ƙarfi (MPa)

7
8
8
8
8
7
Tsawaita(%) 800
850
750
650
500

400

Ƙarfin hawaye (kN/m) 14
20
30
30
22
22





Na baya: 
Na gaba: 

SAUKAR HANYA

KAYANMU

BAYANIN HULDA

Ƙara: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Haƙƙin mallaka     2023 Shanghai Herchy Rubber Co., Ltd. Taswirar yanar gizo |   Manufar Keɓantawa | Taimako Ta Leadong.