GA-71×
Herchy
| Upatikanaji: | |
|---|---|
| Kiasi: | |
Jaribio: 1% ya kikali ya kuponya (50% ya kuweka DBPMH ins小conegum), 175° x 5min x 15MPa.
| Vigezo vya bidhaa | ||||||
| Bidhaa | GA-7120 |
GA-7130 | GA-7131 | GA-7151 | GA-7161 | GA-7171 |
| Muonekano | Uwazi | |||||
| Williamplasticity |
140 |
160 |
200 |
220 |
240 |
280 |
| Ugumu (ShoreA) |
25 |
30 |
40 |
50 |
60 |
70 |
| Msongamano(g/cm3) | 1.10 |
1.12 |
1.14 |
1.18 |
1.20 |
1.23 |
| Nguvu ya mkazo (MPa) |
7 |
8 |
8 |
8 |
8 |
7 |
| Kurefusha(%) | 800 |
850 |
750 |
650 |
500 |
400 |
| Nguvu ya machozi (kN/m) | 14 |
20 |
30 |
30 |
22 |
22 |