GA-71×× Silicone fingotra ho an'ny famolahana amin'ny tanjaky ny ranomaso avo (HCR)

Fampiharana: karazana saron-tava rehetra, kitapom-batsy, fehin-tànana, fingotra, firavaka ary vokatra avo lenta hafa.
Ny endri-javatra lehibe: avo lenta, fanafahana tsara, fahaiza-manao tsara, mandalo ny fanamarinana ny RoHS, REACH, ary FDA.
  • GA-71××

  • Herchy

Availability:
Quantity:

Fitsapana: 1% amin'ny fanafody fanasitranana (50% pasteur DBPMH ins小conegum), 175° x 5min x 15MPa.


Masontsivana vokatra
vokatra GA-7120
GA-7130 GA-7131 GA-7151 GA-7161 GA-7171
Bika Aman 'endrika Translucent
Williamplasticity
140
160
200
220
240
280
Hardness (ShoreA)
25
30
40
50
60
70
Hateza (g/cm3) 1.10
1.12
1.14
1.18
1.20
1.23
Henjana (MPa)

7
8
8
8
8
7
Elongation(%) 800
850
750
650
500

400

Hain-dranomaso (kN/m) 14
20
30
30
22
22





teo aloha: 
Manaraka: 

ROHINY HAINGANA

NY PRODUKY

ANTSIPIRIANY IFANDRAISANA

Add: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Copyright     2023 Shanghai Herchy Rubber Co., Ltd. Sitemap |   Politika momba ny fiainana manokana | Support By Leadong.