GA-71 × × Silicone Roj Hmab rau Moulding nrog Siab Tear Strength (HCR)

Daim ntawv thov: txhua yam sheath, hnab nyiaj, watchband, roj hmab band, hniav nyiaj hniav kub thiab lwm yam khoom muaj zog.
Cov yam ntxwv tseem ceeb: kev kub ntxhov, kev tso tawm zoo, kev ua haujlwm zoo, dhau qhov kev lees paub ntawm RoHS, REACH, thiab FDA.
  • GA-71 × x

  • Herchy

Muaj:
Quantity:

Test: 1% ntawm curing agent (50% paste of DBPMH ins 小conegum), 175° x 5min x 15MPa.


Khoom parameters
Khoom TIAB SA-7120
TIAB SA-7130 TIAB SA-7131 TIAB SA-7151 TIAB SA-7161 TIAB SA-7171
Qhov tshwm sim Translucent
Williamplasticity
140
160
200
220
240
280
Hardness (ShoreA)
25
30
40
50
60
70
Qhov ceev (g / cm3) 1.10
1.12
1.14
1.18
1.20
1.23
Tensilestrength (MPa)

7
8
8
8
8
7
Elongation (%) 800
850
750
650
500

400

Siab zog (kN / m) 14
20
30
30
22
22





Yav dhau los: 
Tom ntej: 

QUICK LINKS

Peb cov khoom

Tiv tauj xov xwm

Ntxiv: No.33, Txoj Kev 159, Taiye Road, Fengxian District, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Copyright     2023 Shanghai Herchy Rubber Co., Ltd. Daim duab qhia chaw |   Txoj Cai Tswjfwm Ntiag Tug | Txhawb nqa By Leadong.