Ujian: 1% agen pengawetan (50% pes DBPMH ins小conegum), 175° x 5min x 15MPa.
| Parameter produk | ||||||
| produk | GA-7120 |
GA-7130 | GA-7131 | GA-7151 | GA-7161 | GA-7171 |
| Penampilan | Lutsinar | |||||
| Williamplasticity |
140 |
160 |
200 |
220 |
240 |
280 |
| Kekerasan (ShoreA) |
25 |
30 |
40 |
50 |
60 |
70 |
| Ketumpatan(g/cm3) | 1.10 |
1.12 |
1.14 |
1.18 |
1.20 |
1.23 |
| Kekuatan tegangan (MPa) |
7 |
8 |
8 |
8 |
8 |
7 |
| Pemanjangan(%) | 800 |
850 |
750 |
650 |
500 |
400 |
| Kekuatan air mata (kN/m) | 14 |
20 |
30 |
30 |
22 |
22 |