GA-71××
Herchy
| kasedhiyan: | |
|---|---|
| Jumlah: | |
Tes: 1% saka agen curing (50% pasta saka DBPMH ins小conegum), 175° x 5min x 15MPa.
| Parameter produk | ||||||
| produk | GA-7120 |
GA-7130 | GA-7131 | GA-7151 | GA-7161 | GA-7171 |
| Penampilan | Tembus | |||||
| Williamplastisitas |
140 |
160 |
200 |
220 |
240 |
280 |
| Kekerasan (ShoreA) |
25 |
30 |
40 |
50 |
60 |
70 |
| Kapadhetan (g/cm3) | 1.10 |
1.12 |
1.14 |
1.18 |
1.20 |
1.23 |
| Daya Tarik (MPa) |
7 |
8 |
8 |
8 |
8 |
7 |
| Elongasi (%) | 800 |
850 |
750 |
650 |
500 |
400 |
| Kekuwatan sobek (kN/m) | 14 |
20 |
30 |
30 |
22 |
22 |