GA-71××, oyo ezali na kati
HERCHY .
| Bozali: | |
|---|---|
| Motango: | |
Momekano: 1% ya agent curing (50% ya pâte ya DBPMH ins小conegum), 175° x 5min x 15MPa.
| Ba paramètres ya produit | ||||||
| Eloko | GA-7120 |
GA-7130 | GA-7131 | GA-7151 | GA-7161 | GA-7171 |
| Komonana | Translucide ezali | |||||
| Williamplasticité ya kosala |
140 |
160 |
200 |
220 |
240 |
280 |
| Bokasi ya makasi (ShoreA) . |
25 |
30 |
40 |
50 |
60 |
70 |
| Densité(g/cm3) Ezali na ba . | 1.10 |
1.12 |
1.14 |
1.18 |
1.20 |
1.23 |
| Bokasi ya kokangama (MPa) . |
7 |
8 |
8 |
8 |
8 |
7 |
| Elongation(%) ya . | 800 |
850 |
750 |
650 |
500 |
400 |
| Bokasi ya mai ya miso (kN/m) . | 14 |
20 |
30 |
30 |
22 |
22 |