GA-30×1
| Availability: | |
|---|---|
| Quantity: | |
Test: 1% of curing agent (50% paste of DBPMH in silicone gum), 175° x5minx15MPa
| Product parameters | |||||||
| Product | GA-3021 | GA-3031 | GA-3041 | GA-3051 | GA-3061 | GA-3071 | GA-3081 |
| Appearance | Translucent | ||||||
| Williamplasticity | 100 | 140 | 180 | 210 | 240 | 280 | 310 |
| Hardness (ShoreA) | 25 | 30 | 40 | 50 | 60 | 70 | 80 |
| Density(g/cm3) | 1.08 | 1.08 | 1.11 | 1.14 | 1.17 | 1.20 | 1.22 |
| Tensile strength (MPa) | 6 | 8 | 11 | 11 | 11 | 9 | 8 |
| Elongation(%) | 950 | 900 | 800 | 700 | 600 | 400 | 200 |
| Tear strength (kN/m) | 12 | 18 | 22 | 25 | 30 | 30 | 22 |