GA-30×1
| Beskikberens: | |
|---|---|
| Kwantiteit: | |
Test: 1% kurermiddel (50% pasta fan DBPMH yn silikongum), 175 ° x5minx15MPa
| Produkt parameters | |||||||
| Produkt | GA-3021 |
GA-3031 | GA-3041 | GA-3051 | GA-3061 | GA-3071 | GA-3081 |
| Ferskining | Trochsichtich | ||||||
| Williamplasticity |
100 |
140 |
180 |
210 |
240 |
280 |
310 |
| Hardheid (ShoreA) |
25 |
30 |
40 |
50 |
60 |
70 |
80 |
| Tichtheid (g/cm3) | 1.08 |
1.08 |
1.11 |
1.14 |
1.17 |
1.20 |
1.22 |
| Treksterkte (MPa) |
6 |
8 |
11 |
11 |
11 |
9 |
8 |
| Ferlinging (%) | 950 |
900 |
800 |
700 |
600 |
400 |
200 |
| Tear sterkte (kN/m) | 12 |
18 |
22 |
25 |
30 |
30 |
22 |