GA-30×1
| Loaʻa: | |
|---|---|
| Nui: | |
Ho'āʻo: 1% o ka lāʻau lapaʻau (50% paʻi o DBPMH i ka silicone gum), 175° x5minx15MPa
| Nā palena huahana | |||||||
| Huahana | GA-3021 |
GA-3031 | GA-3041 | GA-3051 | GA-3061 | GA-3071 | GA-3081 |
| Ka nana aku | Alohilohi | ||||||
| Williamplasticity |
100 |
140 |
180 |
210 |
240 |
280 |
310 |
| Paʻakikī (ShoreA) |
25 |
30 |
40 |
50 |
60 |
70 |
80 |
| Māmā (g/cm3) | 1.08 |
1.08 |
1.11 |
1.14 |
1.17 |
1.20 |
1.22 |
| Ka ikaika uʻi (MPa) |
6 |
8 |
11 |
11 |
11 |
9 |
8 |
| Elongation(%) | 950 |
900 |
800 |
700 |
600 |
400 |
200 |
| Kaha waimaka (kN/m) | 12 |
18 |
22 |
25 |
30 |
30 |
22 |