GA-30 × 1 Silicone pa'u mo le fa'aliliina (fumed silica) fa'atasi ai ma mea lelei e tete'e samasama (HCR)

Fa'aaogāga: 'ese'ese ituaiga o fa'afu, umukuka, ato, fusi ma isi mea, lea e mana'omia ai mea lelei fa'atosina-samasama.
Fa'ailoga autu: maualuga le malosi, maualuga le manino, lelei le faagasologa, pasi le faʻamaoniga o le RoHS, REACH, ma le LFGB.
  • GA-30×1

Avanoa:
Aofaiga:

Su'ega: 1% o le vaila'au fa'amalolo (50% fa'apipi'i o le DBPMH i le pulu silicone), 175° x5minx15MPa


Fa'atauga o oloa
Oloa GA-3021
GA-3031 GA-3041 GA-3051 GA-3061 GA-3071 GA-3081
Fa'aaliga Translucent
Williamplasticity
100
140
180
210
240
280
310
Malosi (ShoreA)
25
30
40
50
60
70
80
Malosi (g/cm3) 1.08
1.08
1.11
1.14
1.17
1.20
1.22
Malosi fa'amalosi (MPa)

6
8
11
11
11
9
8
Fa'atele(%) 950
900
800
700
600
400
200
Malosi o loimata (kN/m) 12
18
22
25
30
30
22







Muamua: 
Sosoo ai: 

SO'OGA VAIVAI

OA TATOU Oloa

FA'AMATALAGA FESOASOANI

Faʻaopoopo: Nu.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Telefoni / WhatsApp / Skype: +86 15221953351
Puletaofia     2023 Shanghai Herchy Rubber Co., Ltd. Sitemap |   Faiga Fa'alilolilo | Lagolago e Leadong.