GA-30×1 ye
| A sɔrɔli: | |
|---|---|
| Hakɛ: . | |
Kɔrɔbɔli : 1% furakɛlifɛn (DBPMH 50% paste silikɔni gomu kɔnɔ), 175° x5minx15MPa
| Fɛn dilannenw ka paramɛtiriw | |||||||
| Ka kɛ | GA-3021 ye |
GA-3031 ye | GA-3041 ye | GA-3051 ye | GA-3061 ye | GA-3071 ye | GA-3081 ye |
| Yecogo | Translucent (yɔrɔ jɛlen) ye | ||||||
| Williamplasticity (Wiliamplasticité) ye |
100 |
140 |
180 |
210 |
240 |
280 |
310 |
| Gɛlɛya (KɔgɔjidaA) . |
25 |
30 |
40 |
50 |
60 |
70 |
80 |
| Densité(g/cm3) ye. | 1.08 |
1.08 |
1.11 |
1.14 |
1.17 |
1.20 |
1.22 |
| Sɛgɛsɛgɛli fanga (MPa) . |
6 |
8 |
11 |
11 |
11 |
9 |
8 |
| Janya(%) . | 950 |
900 |
800 |
700 |
600 |
400 |
200 |
| Ɲɛjibɔ fanga (kN/m) . | 12 |
18 |
22 |
25 |
30 |
30 |
22 |