GA-30 × 1 Rubber ya silicone yo kubumba (silika fumed) hamwe nibintu byiza birwanya umuhondo (HCR)

Gushyira mu bikorwa: ubwoko butandukanye bwicyatsi, ibikoresho byo mu gikoni, isakoshi, umurongo wogukurikirana nibindi, bisaba umutungo mwiza wo kurwanya umuhondo.
Ibyingenzi byingenzi: imbaraga nyinshi, gukorera mu mucyo, gutunganya neza, gutambutsa ibyemezo bya RoHS, REACH, na LFGB.
  • GA-30 × 1

Kuboneka:
Umubare:

Ikizamini: 1% yumuti ukiza (50% paste ya DBPMH mumase ya silicone), 175 ° x5minx15MPa


Ibipimo byibicuruzwa
Ibicuruzwa GA-3021
GA-3031 GA-3041 GA-3051 GA-3061 GA-3071 GA-3081
Kugaragara Birasobanutse
Yamamoto
100
140
180
210
240
280
310
Gukomera (ShoreA)
25
30
40
50
60
70
80
Ubucucike (g / cm3) 1.08
1.08
1.11
1.14
1.17
1.20
1.22
Imbaraga zingana (MPa)

6
8
11
11
11
9
8
Kurambura (%) 950
900
800
700
600
400
200
Amarira amarira (kN / m) 12
18
22
25
30
30
22







Mbere: 
Ibikurikira: 

LINKS

IBICURUZWA BYACU

AMAKURU

Ongeraho: No.33, Umuhanda 159, Umuhanda wa Taiye, Akarere ka Fengxian, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Uburenganzira     2023 Shanghai Herchy Rubber Co., Ltd. Ikarita |   Politiki Yibanga | Inkunga Na Kurongora.