GA-30×1
| Helitaanka: | |
|---|---|
| Tirada: | |
Tijaabada: 1% wakiilka daweynta (50% koollada DBPMH ee xanjada silikoonka), 175° x5minx15MPa
| Xuduudaha alaabta | |||||||
| Alaabta | GA-3021 |
GA-3031 | GA-3041 | GA-3051 | GA-3061 | GA-3071 | GA-3081 |
| Muuqashada | Translucent | ||||||
| Williamplasticity |
100 |
140 |
180 |
210 |
240 |
280 |
310 |
| Adag ( ShoreA) |
25 |
30 |
40 |
50 |
60 |
70 |
80 |
| Cufnaanta (g/cm3) | 1.08 |
1.08 |
1.11 |
1.14 |
1.17 |
1.20 |
1.22 |
| Xoog xajin (MPa) |
6 |
8 |
11 |
11 |
11 |
9 |
8 |
| Dheeraynta(%) | 950 |
900 |
800 |
700 |
600 |
400 |
200 |
| Xoogga jeexjeexa (kN/m) | 12 |
18 |
22 |
25 |
30 |
30 |
22 |