GA-30×1
| Beskikbaarheid: | |
|---|---|
| Hoeveelheid: | |
Toets: 1% verhardingsmiddel (50% pasta van DBPMH in silikoongom), 175° x5minx15MPa
| Produk parameters | |||||||
| Produk | GA-3021 |
GA-3031 | GA-3041 | GA-3051 | GA-3061 | GA-3071 | GA-3081 |
| Voorkoms | Deurskynend | ||||||
| Williamplastisiteit |
100 |
140 |
180 |
210 |
240 |
280 |
310 |
| Hardheid (ShoreA) |
25 |
30 |
40 |
50 |
60 |
70 |
80 |
| Digtheid (g/cm3) | 1.08 |
1.08 |
1.11 |
1.14 |
1.17 |
1.20 |
1.22 |
| Treksterkte (MPa) |
6 |
8 |
11 |
11 |
11 |
9 |
8 |
| Verlenging (%) | 950 |
900 |
800 |
700 |
600 |
400 |
200 |
| Skeursterkte (kN/m) | 12 |
18 |
22 |
25 |
30 |
30 |
22 |