Tel: +8615221953351   E-mail: info@herchyrubber.com
PRODUCTS
You are here: Home » Products » Synthesis Rubber » VMQ Silicone » GA-30×1 Silicone rubber for molding (fumed silica) with good anti-yellowing property (HCR)

loading

Share to:
facebook sharing button
twitter sharing button
line sharing button
wechat sharing button
linkedin sharing button
pinterest sharing button
whatsapp sharing button
sharethis sharing button

GA-30×1 Silicone rubber for molding (fumed silica) with good anti-yellowing property (HCR)

Application: various kinds of sheath, kitchenware, purse, watchband and so on, whichrequire good anti-yellowing property.
Key features: high strength, high transparence, excellent processability, pass theauthentication of RoHS, REACH, and LFGB.
  • GA-30×1

Availability:
Quantity:

Test: 1% of curing agent (50% paste of DBPMH in silicone gum), 175° x5minx15MPa


Product parameters
ProductGA-3021
GA-3031GA-3041GA-3051GA-3061GA-3071GA-3081
AppearanceTranslucent
Williamplasticity
100
140
180
210
240
280
310
Hardness (ShoreA)
25
30
40
50
60
70
80
Density(g/cm3)1.08
1.08
1.11
1.14
1.17
1.20
1.22
Tensile strength (MPa)

6
8
11
11
11
9
8
Elongation(%)950
900
800
700
600
400
200
Tear strength (kN/m)12
18
22
25
30
30
22







Previous: 
Next: 

QUICK LINKS

OUR PRODUCTS

CONTACT INFORMATION

Add: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Tel / WhatsApp / Skype: +8615221953351
Copyright  2023 Shanghai Herchy Rubber Co., Ltd. Sitemap |  Privacy Policy | Support By Leadong.