GA-28X0 High_ Strength LSR (LSR)

Aplikasi: cocok kanggo ngasilake produk pawon, segel kanggo keperluan industri, mesin cuci lan barang-barang liyane.
Fitur utama: kekuatan dhuwur, bahan pangan, lulus otentikasi RoHS, REACH, FDA lan LFGB.
  • GA-2820

  • Herchy

kasedhiyan:
Jumlah:

Tes: rasio A/B 1:1, 130°C x 5min x 15MPa


Parameter produk
produk GA-2820 GA-2830 GA-2840 GA-2850 GA-2860 GA-2870
Penampilan Tembus

Viskositas (Pa)
2000 2500 3000 3500 4000 4000
Kekerasan (ShoreA) 20 30 40 50
60
70
Kapadhetan (g/cm3) 1.10 1.10 1.11 1.12 1.13
1.14
Kekuatan tarik (MPa) 6.5
7.5
9.0
9.5
9.5
9.0
Elongasi (%) 850 780 650 500 400
300
Kekuwatan sobek (kN/m) 12 15 30 35 30
30
Linearshrinkage(%) 2.1 2.1 2.1 2.0 2.0
2.0






Sadurunge: 
Sabanjure: 

LINKS CEPAT

PRODUK KAMI

INFORMASI KONTAK

Tambah: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Telpon / WhatsApp / Skype: +86 15221953351
Hak Cipta     2023 Shanghai Herchy Rubber Co., Ltd. Sitemap |   Kebijakan Privasi | Dhukungan dening Leadong.