GA-2820
Herchy
| Wātea: | |
|---|---|
| Rahi: | |
Whakamātautau: A/B ōwehenga o 1 :1, 130°C x 5min x 15MPa
| Tawhā hua | |||||||
| Hua | GA-2820 | GA-2830 | GA-2840 | GA-2850 | GA-2860 | GA-2870 | |
| Te ahua | Puatarangi | ||||||
| Viscosity(Pa.s) |
2000 | 2500 | 3000 | 3500 | 4000 | 4000 |
|
| Maama (ShoreA) | 20 | 30 | 40 | 50 |
60 |
70 |
|
| Kiato(g/cm3) | 1.10 | 1.10 | 1.11 | 1.12 | 1.13 |
1.14 |
|
| Te kaha o te kaha (MPa) | 6.5 |
7.5 |
9.0 |
9.5 |
9.5 |
9.0 |
|
| Whakaroa(%) | 850 | 780 | 650 | 500 | 400 |
300 |
|
| Te kaha roimata (kN/m) | 12 | 15 | 30 | 35 | 30 |
30 |
|
| Te whakahekenga raina(%) | 2.1 | 2.1 | 2.1 | 2.0 | 2.0 |
2.0 |
|