GA-2820 irratti kan hundaa’e
Herchy jedhamuun beekama
| Argamuu: | |
|---|---|
| Baay’ina: | |
Qormaata: Reeshiyoon A/B 1 :1, 130°C x 5min x 15MPa
| Parameetaroota oomishaa | |||||||
| Oomisha | GA-2820 irratti kan hundaa’e | GA-2830 irratti kan argamu | GA-2840 irratti kan argamu | GA-2850 irratti kan argamu | GA-2860 irratti kan argamu | GA-2870 irratti kan argamu | |
| Mul'ina | Kan ifa ta’e | ||||||
| Viskoositii(Pa.s) 1.1. |
2000 | 2500 | 3000 | 3500 | 4000 | 4000 |
|
| Jabina (ShoreA) . | 20 | 30 | 40 | 50 |
60 |
70 |
|
| Dandeettii(g/cm3) . | 1.10 | 1.10 | 1.11 | 1.12 | 1.13 |
1.14 |
|
| Jabina harkisaa (MPa) . | 6.5 |
7.5 |
9.0 |
9.5 |
9.5 |
9.0 |
|
| Dheersuu(%) . | 850 | 780 | 650 | 500 | 400 |
300 |
|
| Jabina ciccituu (kN/m) . | 12 | 15 | 30 | 35 | 30 |
30 |
|
| Sarara xiqqaachuu(%) . | 2.1 | 2.1 | 2.1 | 2.0 | 2.0 |
2.0 |
|