GA- 2820
Herchy
| Argaeledd: | |
|---|---|
| Nifer: | |
Prawf: Cymhareb A/B o 1:1, 130°C x 5min x 15MPa
| Paramedrau cynnyrch | |||||||
| Cynnyrch | GA- 2820 | GA- 2830 | GA- 2840 | GA- 2850 | GA- 2860 | GA- 2870 | |
| Ymddangosiad | Tryleu | ||||||
| Gludedd (Pas) |
2000 | 2500 | 3000 | 3500 | 4000 | 4000 |
|
| Caledwch (ShoreA) | 20 | 30 | 40 | 50 |
60 |
70 |
|
| Dwysedd(g/cm3) | 1.10 | 1.10 | 1.11 | 1.12 | 1.13 |
1.14 |
|
| Cryfder tynnol (MPa) | 6.5 |
7.5 |
9.0 |
9.5 |
9.5 |
9.0 |
|
| elongation(%) | 850 | 780 | 650 | 500 | 400 |
300 |
|
| Cryfder dagrau (kN/m) | 12 | 15 | 30 | 35 | 30 |
30 |
|
| crebachu llinol (%) | 2.1 | 2.1 | 2.1 | 2.0 | 2.0 |
2.0 |
|