GA-2820
Herchy
| Availability: | |
|---|---|
| Quantity: | |
Test: A/B proportio 1 :1, 130°C x 5min x 15MPa
| Product parametri | |||||||
| Productum | GA-2820 | GA-2830 | GA-2840 | GA-2850 | GA-2860 | GA-2870 | |
| Aspectus | Translucens | ||||||
| Viscositas (Pa.s) |
2000 | 2500 | 3000 | 3500 | 4000 | 4000 |
|
| Duritia (ShoreA) | 20 | 30 | 40 | 50 |
60 |
70 |
|
| Densitas (g/cm3) | 1.10 | 1.10 | 1.11 | 1.12 | 1.13 |
1.14 |
|
| Roboris distrahentes (MPa) | 6.5 |
7.5 |
9.0 |
9.5 |
9.5 |
9.0 |
|
| Prolongatio(%) | 850 | 780 | 650 | 500 | 400 |
300 |
|
| Robur scindere (kN/m) | 12 | 15 | 30 | 35 | 30 |
30 |
|
| Linearshrinkage(%) | 2.1 | 2.1 | 2.1 | 2.0 | 2.0 |
2.0 |
|