Test: A/B-verhouding van 1:1, 130°C x 5min x 15MPa
| Productparameters | |||||||
| Product | GA-2820 | GA-2830 | GA-2840 | GA-2850 | GA-2860 | GA-2870 | |
| Verschijning | Doorschijnend | ||||||
| Viscositeit (Pa.s) |
2000 | 2500 | 3000 | 3500 | 4000 | 4000 |
|
| Hardheid (ShoreA) | 20 | 30 | 40 | 50 |
60 |
70 |
|
| Dichtheid (g/cm3) | 1.10 | 1.10 | 1.11 | 1.12 | 1.13 |
1.14 |
|
| Treksterkte (MPa) | 6.5 |
7.5 |
9.0 |
9.5 |
9.5 |
9.0 |
|
| Verlenging (%) | 850 | 780 | 650 | 500 | 400 |
300 |
|
| Scheursterkte (kN/m) | 12 | 15 | 30 | 35 | 30 |
30 |
|
| Lineaire krimp (%) | 2.1 | 2.1 | 2.1 | 2.0 | 2.0 |
2.0 |
|