GA- 2820
Earcach
| Infhaighteacht: | |
|---|---|
| Cainníocht: | |
Tástáil: Cóimheas A/B de 1:1, 130°C x 5min x 15MPa
| Paraiméadair táirge | |||||||
| Táirge | GA- 2820 | GA- 2830 | GA- 2840 | GA- 2850 | GA- 2860 | GA-2870 | |
| Dealramh | Tréshoilseach | ||||||
| Slaodacht(Pas) |
2000 | 2500 | 3000 | 3500 | 4000 | 4000 |
|
| Cruas (ShoreA) | 20 | 30 | 40 | 50 |
60 |
70 |
|
| Dlús(g/cm3) | 1.10 | 1.10 | 1.11 | 1.12 | 1.13 |
1.14 |
|
| Neart teanntachta (MPa) | 6.5 |
7.5 |
9.0 |
9.5 |
9.5 |
9.0 |
|
| Fadú(%) | 850 | 780 | 650 | 500 | 400 |
300 |
|
| Neart cuimilt (kN/m) | 12 | 15 | 30 | 35 | 30 |
30 |
|
| Laghdaigh líneach(%) | 2.1 | 2.1 | 2.1 | 2.0 | 2.0 |
2.0 |
|