GA-28X0 ƝƐNAJƐ NI ƝƐNAJƐW ƝƐNAJƐW .

A kɛcogo: a bɛnnen don ka dumunikɛminɛnw dilan, sigilan minnu bɛ kɛ iziniw kɔnɔ, kolikɛnɛw ani fɛn suguya wɛrɛw.
Fɛn kolomaw : fanga ka bon, dumuni hakɛ, tɛmɛ RoHS, REACH,FDA ani LFGB tiɲɛni na.
  • GA-2820 ye

  • Herchy .

A sɔrɔli:
Hakɛ: .

Kɔrɔbɔli : A/B hakɛ ye 1 :1 ye, 130°C x 5min x 15MPa


Product Paramɛtɛrɛw .
Ka kɛ GA-2820 ye GA-2830 ye GA-2840 ye GA-2850 ye GA-2860 ye GA-2870 ye
Yecogo Translucent .

Viscosité(Pa.s) ka .
2000 2500 3000 3500 4000 4000
Gɛlɛya (Shoaa) . 20 30 40 50
60
70
Densité(g/cm3) ye. 1.10 1.10 1.11 1.12 1.13
1.14
Sɛgɛsɛgɛli fanga (MPa) . 6.5
7.5
9.0
9.5
9.5
9.0
Janya(%) . 850 780 650 500 400
300
Ɲɛjibɔ fanga (KN/M) . 12 15 30 35 30
30
Linearshrinkage(%) Bamako, Mali. 2.1 2.1 2.1 2.0 2.0
2.0






Tɛmɛnen: 
Nata: 

LINKS TELIKANW

An ka fɛn dilannenw .

KUNNAFONIW MINNU BƐ SƆRƆ

A farala: No.33, Lane 159, Taiye sira kan, Fengxian mara la, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Hakilila-jɔ-sɛbɛn     2023 Shanghai Herchy Rubber Co., Ltd. Sitemap (yɔrɔ karti). |   Kunnafoni dogolenw ka sariya | Dɛmɛn By Leadong ye.