GA-28X0 Phahameng_ Matla LSR (LSR) .

Kopo: e loketseng bakeng sa ho hlahisa dihlahiswa kichineng, ditiiso bakeng sa tshebediso ya indasteri, washersand dintho tse ling tse fapa-fapaneng.
Key litšobotsi: matla phahameng, lijo sehlopha, feta netefatso ea RoHS, REACH,FDA le LFGB.
  • GA-2820 ya go swana le yona

  • Herchy ya go swana le

Go hwetšagala:
Palo: .

Teko: A / B karo-karolelano ya 1 :1, 130 ° C x 5min x 15MPa


Ditekanyetšo tša setšweletšwa
Setšweletšwa GA-2820 ya go swana le yona GA-2830 ya go swana le yona GA-2840 ya go swana le yona GA-2850 ya go swana le yona GA-2860 ya go swana le yona GA-2870 ya go swana le yona
Ponagalo E translucent

Sekgomaretši(Pa.s) .
2000 2500 3000 3500 4000 4000
Thata (LebopoA) . 20 30 40 50
60
70
Kitlano (g / cm3) . 1.10 1.10 1.11 1.12 1.13
1.14
Matla a go goga (MPa) . 6.5
7.5
9.0
9.5
9.5
9.0
Go telefatšwa(%) . 850 780 650 500 400
300
Matla a go gagola (kN/m) . 12 15 30 35 30
30
Go fokotšega ga mothalo(%) . 2.1 2.1 2.1 2.0 2.0
2.0






Peleng: 
Latelago: 

DIKGOKAGANO TŠA KA PELE

DIHLAHISWA TSA RONA

TSHEDIMOŠO YA KGOKAGANO

Add: No.33, Lane 159, Tsela ya Taiye, Setereke sa Fengxian, Shanghai
Mogala / WhatsApp / Skype: +86 15221953351 Mogala wa Sepedi
Tokelo ya ngwalollo e ileditšwe     2023 Shanghai Herchy Rabara Co., Ltd. Mmapa wa Sebaka |   Pholisi ya Sephiri | Thekgo Ka Leadong ya go iša.