GA-2820 we dɛn kɔl
Herchy bin de du am
| Di tin dɛn we yu kin gɛt: | |
|---|---|
| Kwantiti: . | |
Test: A/B ratio fɔ 1 :1, 130°C x 5min x 15MPa
| Prodakt paramita dɛn | |||||||
| Sɔntin | GA-2820 we dɛn kɔl | GA-2830 we dɛn kɔl | GA-2840 we dɛn kɔl | GA-2850 we dɛn kɔl | GA-2860 we dɛn kɔl | GA-2870 we dɛn kɔl | |
| Aw a luk | Translucent we de mek pɔsin fil fayn | ||||||
| Viskositi(Pa.s) . |
2000 | 2500 | 3000 | 3500 | 4000 | 4000 |
|
| Di hadnɛs (ShoreA) . | 20 | 30 | 40 | 50 |
60 |
70 |
|
| Densiti(g/cm3) . | 1.10 | 1.10 | 1.11 | 1.12 | 1.13 |
1.14 |
|
| Tensile strɛngth (MPa) . | 6.5 |
7.5 |
9.0 |
9.5 |
9.5 |
9.0 |
|
| Elongation(%) we de go bifo. | 850 | 780 | 650 | 500 | 400 |
300 |
|
| Tear strɛngth (kN/m) . | 12 | 15 | 30 | 35 | 30 |
30 |
|
| Linearshrinkage(%) we de sכmtεm . | 2.1 | 2.1 | 2.1 | 2.0 | 2.0 |
2.0 |
|