GA-2430 LSR ee Dahaarka dabacsan (LSR)

Codsiga: ku habboon soo saarista daahan fiber galaas, daahan iyo alaabta isbuunyada, iwm.
Astaamaha muhiimka ah: xoog wanaagsan, isku xirnaan adag, xawaare daaweyn degdeg ah.
  • GA-2430

  • Herchy

Helitaanka:
Tirada:

Tijaabada: Saamiga A/B waa la hagaajin karo, 130°Cx 5min x 15MPa.


Xuduudaha alaabta
Alaabta GA-2430 GA-2440 GA-2450
Muuqashada Translucent
A/B配比A/Bratio 2:100
2:100
2:100
B剂粘度 Viscosity of part-B (Pa·s)
10-200 10-200 10-200
Adag ( ShoreA) 28 38
50
Cufnaanta (g/cm3)

1.08

1.06 1.10
Xoog xajin (MPa) 4.0
4.5
7.0
Dheeraynta(%) 300 250 350
Xoogga jeexjeexa (kN/m) 10 15 15
Hoos u dhac toos ah (%) 2.1 2.1
2.0









Kii hore: 
Xiga: 

XIDHIIDHYADA DEGDEGGA AH

Alaabooyinkayaga

MACLUUMAADKA XIRIIRKA

Kudar: No.33, Lane 159, Wadada Taiye, Degmada Fengxian, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Xuquuqda daabacaadda     2023 Shanghai Herchy Rubber Co., Ltd. Khariidadda goobta |   Siyaasadda Qarsoonnimada | Taageerada By Leadong.