Moslashuvchan qoplama uchun GA-2430 LSR (LSR)

Ilova: shisha tolali qoplama, qoplama va shimgichni ishlab chiqarish uchun javob beradi.
Asosiy xususiyatlar: yaxshi quvvat, kuchli bog'lanish, tez quritish tezligi.
  • GA-2430

  • Herchi

Mavjudligi:
Miqdori:

Sinov: A/B nisbati sozlanishi, 130°Cx 5min x 15MPa.


Mahsulot parametrlari
Mahsulot GA-2430 GA-2440 GA-2450
Tashqi ko'rinish Shaffof
A/BlíníA/Bratio 2:100
2:100
2:100
B-qismining yopishqoqligi (Pa·s)
10-200 10-200 10-200
Qattiqlik (ShoreA) 28 38
50
Zichlik (g/sm3)

1.08

1.06 1.10
Kuchlanish kuchi (MPa) 4.0
4.5
7.0
Uzayish (%) 300 250 350
Yirilish kuchi (kN/m) 10 15 15
Chiziqli qisqarish (%) 2.1 2.1
2.0









Oldingi: 
Keyingisi: 

TEZKOR havolalar

MAHSULOTLARIMIZ

BOG'LANISH UCHUN MA'LUMOT

Qo'shish: №33, 159-ko'cha, Taiye yo'li, Fengxian tumani, Shanxay
Tel / WhatsApp / Skype: +86 15221953351
Mualliflik huquqi     2023 Shanghai Herchy Rubber Co., Ltd. Sayt xaritasi |   Maxfiylik siyosati | Qo'llab-quvvatlash Leadong.