Kɔrɔbɔli: A/B hakɛ bɛ se ka ladilan, 130°Cx 5min x 15MPa.
| Fɛn dilannenw ka paramɛtiriw | ||||
| Ka kɛ | GA-2430 ye | GA-2440 ye | GA-2450 ye | |
| Yecogo | Translucent (yɔrɔ jɛlen) ye | |||
| A/B配比A/Bratio ye a ka baara ye | 2:100 la |
2:100 la |
2:100 la |
|
| B剂粘度Bi yɔrɔ-B (Pa·s) ka sɔgɔsɔgɔninjɛ . |
10-200 kɔnɔ | 10-200 kɔnɔ | 10-200 kɔnɔ | |
| Gɛlɛya (KɔgɔjidaA) . | 28 | 38 |
50 |
|
| Densité(g/cm3) ye. | 1.08 |
1.06 | 1.10 | |
| Sɛgɛsɛgɛli fanga (MPa) . | 4.0 |
4.5 |
7.0 |
|
| Janya(%) . | 300 | 250 | 350 | |
| Ɲɛjibɔ fanga (kN/m) . | 10 | 15 | 15 | |
| Linearshrinkage(%) Bamako, Mali. | 2.1 | 2.1 |
2.0 |
|