GA-2430 LSR no ka uhi hikiwawe (LSR)

Noi: kūpono no ka hana ʻana i ka uhi aniani fiber, ka uhi a me nā huahana sponge, etc.
ʻO nā hiʻohiʻona nui: ikaika maikaʻi, hoʻopaʻa paʻa, wikiwiki wikiwiki.
  • GA-2430

  • Herchy

Loaʻa:
Nui:

Ho'āʻo: Hiki ke hoʻololi ʻia ka lakio A/B, 130°Cx 5min x 15MPa.


Nā palena huahana
Huahana GA-2430 GA-2440 GA-2450
Ka nana aku Alohilohi
A/B配比A/Bratio 2:100
2:100
2:100
B剂粘度 ʻO ka viscosity o ka hapa-B (Pa·s)
10-200 10-200 10-200
Paʻakikī (ShoreA) 28 38
50
Māmā (g/cm3)

1.08

1.06 1.10
Ka ikaika uʻi (MPa) 4.0
4.5
7.0
Elongation(%) 300 250 350
Kaha waimaka (kN/m) 10 15 15
Hoʻemi laina (%) 2.1 2.1
2.0









Mua: 
Aʻe: 

NUI WIWIKI

KO MAKOU HANA

IKE HOPE

Hoʻohui: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
leka uila:  info@herchyrubber.com
Kuleana kope     2023 Shanghai Herchy Rubber Co., Ltd. Palapala kahua |   Kulekele pilikino | Kākoʻo Na Leadong.