GA-2430 oyo ezali na kati
Herchy na likambo yango
| Bozali: | |
|---|---|
| Motango: | |
Momekano: Rapport A/B ezali réglable, 130°Cx 5min x 15MPa.
| Ba paramètres ya produit | ||||
| Eloko | GA-2430 oyo ezali na kati | GA-2440 oyo ezali na kati | GA-2450 oyo ezali na kati | |
| Komonana | Translucide ezali | |||
| A/B配比A/Bratio oyo ezali na kati | 2:100 |
2:100 |
2:100 |
|
| B剂粘度Viscosité ya eteni-B (Pa·s) . |
10-200 | 10-200 | 10-200 | |
| Bokasi ya makasi (ShoreA) . | 28 | 38 |
50 |
|
| Densité(g/cm3) Ezali na ba . | 1.08 |
1.06 | 1.10 | |
| Bokasi ya kokangama (MPa) . | 4.0 |
4.5 |
7.0 |
|
| Elongation(%) ya . | 300 | 250 | 350 | |
| Bokasi ya kopasola (kN/m) . | 10 | 15 | 15 | |
| Bokiti ya linéaire(%) . | 2.1 | 2.1 |
2.0 |
|