GA-2430 LSR ad Flexibile Coating (LSR)

Applicatio: apta ad efficiendum vitreum fibra coatingit, efficiens et spongeproducta, etc.
Clavis lineamenta: bonum robur, validum vinculum, celeriter sanans celeritatem.
  • GA-2430

  • Herchy

Availability:
Quantity:

Test: A/B ratio aptabilis, 130°Cx 5min x 15MPa.


Product parametri
Productum GA-2430 GA-2440 GA-2450
Aspectus Translucens
A/B配比A/Bratio 2:100
2:100
2:100
B剂粘度 Viscositas partis B (Pa·s)
10-200 10-200 10-200
Duritia (ShoreA) 28 38
50
Densitas (g/cm3)

1.08

1.06 1.10
Roboris distrahentes (MPa) 4.0
4.5
7.0
Prolongatio(%) 300 250 350
Robur scindere (kN/m) 10 15 15
Linearshrinkage(%) 2.1 2.1
2.0









Priora: 
Next: 

ORIGINAL LINKS

Our Products

Contact Information

Add: No.33, Lane CLIX, Taiye via, Fengxian District, Shanghai
Tel / whatsapp / Skype: +86 15221953351
Copyright     2023 Shanghai Herchy Flexilis Co., Ltd. Sitemap |   Privacy Policy | Support By Leadong.