GA-2430 LSR for Flexible Coating (LSR)

Application: suitable for producing glass fiber coating, coating and spongeproducts, etc.
Key features: good strength,strong bonding, fast curing speed.
  • GA-2430

  • Herchy

Availability:
Quantity:

Test: A/B ratio is adjustable, 130°Cx 5min x 15MPa.


Product parameters
ProductGA-2430GA-2440GA-2450
AppearanceTranslucent
A/B配比A/Bratio2:100
2:100
2:100
B剂粘度Viscosity of part-B (Pa·s)
10-20010-20010-200
Hardness (ShoreA)2838
50
Density(g/cm3)

1.08

1.061.10
Tensile strength (MPa)4.0
4.5
7.0
Elongation(%)300250350
Tear strength (kN/m)101515
Linearshrinkage(%)2.12.1
2.0









Previous: 
Next: 

QUICK LINKS

OUR PRODUCTS

CONTACT INFORMATION

Add: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Tel / WhatsApp / Skype: +8615221953351
Copyright  2023 Shanghai Herchy Rubber Co., Ltd. Sitemap |  Privacy Policy | Support By Leadong.