Sɔhwɛ: A / B ratio yɛ nsakrae, 130 ° Cx 5min x 15MPa.
| Nneɛma a wɔyɛ no parameters | ||||
| Adwadeɛ | GA-2430 na ɛwɔ hɔ | GA-2440 na ɛwɔ hɔ | GA-2450 na ɛwɔ hɔ | |
| Mmaeɛ | Ɛyɛ nea ɛyɛ translucent | |||
| A/B配比A/Nkyekyɛmu | 2:100 na ɛwɔ hɔ |
2:100 na ɛwɔ hɔ |
2:100 na ɛwɔ hɔ |
|
| B剂粘度Nneɛma a ɛyɛ den a ɛwɔ ɔfã-B (Pa·s) mu . |
10-200 na ɛwɔ hɔ | 10-200 na ɛwɔ hɔ | 10-200 na ɛwɔ hɔ | |
| Nneɛma a ɛyɛ den (ShoreA) . | 28 | 38 |
50 |
|
| Nsuo a ɛyɛ den(g/cm3) . | 1.08 |
1.06 | 1.10 | |
| Ahoɔden a wɔde twe ade (MPa) . | 4.0 |
4.5 |
7.0 |
|
| Ntrɛwmu(%) . | 300 | 250 | 350 | |
| Ahoɔden a ɛtetew mu (kN/m) . | 10 | 15 | 15 | |
| Ntrɛwmu a ɛkɔ soro(%) . | 2.1 | 2.1 |
2.0 |
|