GA-2430
Herchy nga bwe kiri
| Ebiriwo: | |
|---|---|
| Omuwendo: | |
Okugezesa: Omugerageranyo gwa A/B gutereezebwa, 130°Cx 5min x 15MPa.
| Ebipimo by’ebintu ebikolebwa | ||||
| Ekyamaguzi | GA-2430 | GA-2440 | GA-2450 | |
| Endabika | Etangalijja | |||
| A/B配比A/Okugatta | 2:100 |
2:100 |
2:100 |
|
| B剂粘度Obuzito bw’ekitundu-B (Pa·s) . |
10-200 | 10-200 | 10-200 | |
| Obukaluba (ShoreA) . | 28 | 38 |
50 |
|
| Obugumu(g/cm3) . | 1.08 |
1.06 | 1.10 | |
| Amaanyi g’okusika (MPa) . | 4.0 |
4.5 |
7.0 |
|
| Okuwanvuwa(%) . | 300 | 250 | 350 | |
| Amaanyi g’okukutuka (kN/m) . | 10 | 15 | 15 | |
| Okukendeera kw’ennyiriri(%) . | 2.1 | 2.1 |
2.0 |
|