GA-2430
Herchy
| Ketersediaan: | |
|---|---|
| Kuantitas: | |
Pengujian: Rasio A/B dapat disesuaikan, 130°Cx 5 menit x 15MPa.
| Parameter produk | ||||
| Produk | GA-2430 | GA-2440 | GA-2450 | |
| Penampilan | Tembus cahaya | |||
| A/B配比A/Brasio | 2:100 |
2:100 |
2:100 |
|
| B剂粘度Viskositas bagian-B (Pa·s) |
10-200 | 10-200 | 10-200 | |
| Kekerasan (ShoreA) | 28 | 38 |
50 |
|
| Massa jenis (g/cm3) | 1.08 |
1.06 | 1.10 | |
| Kekuatan tarik (MPa) | 4.0 |
4.5 |
7.0 |
|
| Pemanjangan(%) | 300 | 250 | 350 | |
| Kekuatan sobek (kN/m) | 10 | 15 | 15 | |
| Penyusutan linier (%) | 2.1 | 2.1 |
2.0 |
|