FVL-7435
Herchy
| Availability: | |
|---|---|
| Quantity: | |
Items |
Test Methods |
NFS-L-7435 |
Appearance A |
visual assessment |
yellowish |
Appearance B |
visual assessment |
yellowish |
Viscosity / Pa.s A (shear rate 10 s-1 ) |
Q/371002WXH028-2016 |
350 |
Viscosity / Pa.s B (shear rate 10 s-1 ) |
Q/371002WXH028-2016 |
300 |
25℃×48h |
||
Specific Gravity/g/cm3 |
ASTM D792 |
1.42 |
Hardness/ShoreA |
ASTM D2240 |
35 |
Tensile Strength/MPa |
ASTM D412 |
8.1 |
Elongation At Break /% |
ASTM D412 |
320 |
Tear Strength/KN/m |
ASTM D624-B |
14.5 |
Resilience/% |
ASTM D1054 |
36 |
Compression Set/%(177℃×22h) |
ASTM D395 |
21 |
Fuel C Volume Change /% (25℃×72h) |
ASTM D471 |
24.0 |
Usage:
NFS-L-7435 liquid fluorosilicone rubber is packed in two-component. When using, A, B components in accordance with the mass ratio of 1:1 mixing and defoaming treatment, room temperature (25 ℃ ± 5 ℃) placed in 48h can be cured completely.
Packing:
Packed in plastic drum, 20kg for each A/B component.
Storage period:
Stored in a cool and dry environment, unopened original packaging storage period of twelve months.
Precautions:
Avoid contact with compounds containing nitrogen, sulphur, phosphorus and heavy metals, which may cause the product to vulcanise uncooked or not vulcanise.