FVL-7435
Herchy
| Availability: | |
|---|---|
| Quantity: | |
Items |
Test Methodi |
NFS-L-7435 |
Aspectus |
visual taxationem |
flavo- |
aspectus B |
visual taxationem |
flavo- |
Viscositas / Pa.s A ( Tondendas rate X s -1 ) |
Q/371002WXH028-2016 |
350 |
Viscositas / Pa.s B ( Tondendas rate X s -1 ) |
Q/371002WXH028-2016 |
300 |
25℃×48h |
||
Imprimis gravitatis / g/cm3 |
ASTM D792 |
1.42 |
Duritiam / ShoreA |
ASTM D2240 |
35 |
Distrahentes Fortitudo / MPa |
ASTM D412 |
8.1 |
Prolongatio In Gaudete /% |
ASTM D412 |
320 |
Lacrima fortitudo/KN/m |
ASTM D624-B |
14.5 |
Mollitia/% |
ASTM D1054 |
36 |
Cogo Set/%(177℃×22h) |
ASTM D395 |
21 |
Cibus C Volumen Mutare /% 25℃×72h) |
ASTM D471 |
24.0 |
Syntaxis:
NFS-L-7435 Flexilis fluorosilicone liquidus in duobus componentibus refertus. Cum utens, A, B, componentibus secundum massam rationi 1, 1 mixtionis et deformandi curationis, locus temperatus (25 ℃ ± 5 ) in 48h positus omnino curari potest.
Stipare:
Tympanum plasticum refertum, 20kg pro singulis componentibus A/B.
Tempus repono:
In ambitu frigido et sicco repositae, originalis tabularii fasciculi periodi duodecim mensium non aperiuntur.
Cautiones:
Fugiat contactum cum compositis nitrogen, sulphure, phosphoro et metallis gravibus, quae causam vulcanise crudi vel non vulcanise efficiunt.