FVL-7435
Herchy nga bwe kiri
| Ebiriwo: | |
|---|---|
| Omuwendo: | |
Ebintu |
Enkola z’okugezesa |
NFS-L-7435 |
Endabika A |
okwekenneenya okulaba |
eya kyenvu |
Endabika B |
okwekenneenya okulaba |
eya kyenvu |
Obuziba / Pa.s A (omuwendo gw’okusala 10 s -1 ) . |
Q/371002WXH028-2016 nga bwe kiri |
350 |
Obuziba / Pa.s B (omuwendo gw’okusala 10 s -1 ) . |
Q/371002WXH028-2016 nga bwe kiri |
300 |
25°C×48h |
||
Obuzito obw’enjawulo/g/cm3 |
ASTM D792 |
1.42 |
Obukaluba/OlubalamaA |
ASTM D2240 nga bwe kiri |
35 |
Amaanyi g’okusika/MPa |
ASTM D412 |
8.1 |
Okuwanvuwa Ku Luwummula /% . |
ASTM D412 |
320 |
Amaanyi g’amaziga/KN/m |
ASTM D624-B |
14.5 |
Obumalirivu/% |
ASTM D1054 nga bwe kiri |
36 |
Okunyigiriza Set/%(177°C×22h) |
ASTM D395 |
21 |
Amafuta C Enkyukakyuka mu ddoboozi /% (25°C×72h) |
ASTM D471 |
24.0 |
Enkozesa:
NFS-L-7435 liquid fluorosilicone rubber epakibwa mu bitundu bibiri. Nga okozesa, ebitundu bya A, B okusinziira ku mugerageranyo gw’obuzito bwa 1:1 okutabula n’okuggyamu eddagala, ebbugumu ly’ekisenge (25 °C ± 5 °C) eriteekeddwa mu 48h liyinza okuwonyezebwa ddala.
Okupakinga:
Epakibwa mu ngoma ya pulasitiika, kkiro 20 ku buli kitundu kya A/B.
Ekiseera ky’okutereka:
Eterekebwa mu mbeera ennyogovu era enkalu, ekiseera ky’okutereka ekipakiddwa ekyasooka nga tekigguddwawo kya myezi kkumi n’ebiri.
Okwegendereza:
Weewale okukwatagana n’ebirungo ebirimu nayitrojeni, salufa, phosphorus n’ebyuma ebizito, ekiyinza okuvaako ekintu okufuuka vulcanize nga tekifumbiddwa oba nga tekifumbiddwa.