FVL-7435 Liquid Fluorosilicone

FVL-7435 Liquid Fluorosilicone Rubber has excellent resistance to high and low temperatures, oil resistance and electrical insulation, and can be cured at room temperature.
  • FVL-7435

  • Herchy

Availability:
Quantity:

Product Performance

Items

Test Methods

NFS-L-7435

Appearance A

visual assessment

yellowish

Appearance B

visual assessment

yellowish

Viscosity / Pa.s A

(shear rate 10 s-1 )

Q/371002WXH028-2016

350

Viscosity / Pa.s B

(shear rate 10 s-1 )

Q/371002WXH028-2016

300

25℃×48h

Specific Gravity/g/cm3

ASTM D792

1.42

Hardness/ShoreA

ASTM D2240

35

Tensile Strength/MPa

ASTM D412

8.1

Elongation At Break /%

ASTM D412

320

Tear Strength/KN/m

ASTM D624-B

14.5

Resilience/%

ASTM D1054

36

Compression Set/%(177℃×22h)

ASTM D395

21

Fuel C

Volume Change /%

(25℃×72h)

ASTM D471

24.0

Usage:

NFS-L-7435 liquid fluorosilicone rubber is packed in two-component. When using, A, B components in accordance with the mass ratio of 1:1 mixing and defoaming treatment, room temperature (25 ℃ ± 5 ℃) placed in 48h can be cured completely.

Packing:

Packed in plastic drum, 20kg for each A/B component.

Storage period:

Stored in a cool and dry environment, unopened original packaging storage period of twelve months.

Precautions:

Avoid contact with compounds containing nitrogen, sulphur, phosphorus and heavy metals, which may cause the product to vulcanise uncooked or not vulcanise.

Previous: 
Next: 

QUICK LINKS

OUR PRODUCTS

CONTACT INFORMATION

Add: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Tel / WhatsApp / Skype: +8615221953351
Copyright  2023 Shanghai Herchy Rubber Co., Ltd. Sitemap |  Privacy Policy | Support By Leadong.