FV9500
Herchy
| Availability: | |
|---|---|
| Quantity: | |
Technical indicators
Items | Indicators | ||||
Grade | FV9540 | FV9550 | FV9560 | FV9561 | |
Appearance Test Methods | yellowish | ||||
Specific Gravity/ g/cm3 | ASTM D792 | 1.40 | 1.41 | 1.42 | 1.44 |
Hardness/shoreA | ASTM D2240 | 41 | 50 | 60 | 61 |
Tensile Strength/MPa | ASTM D412 | 9.5 | 9.8 | 10.2 | 9.8 |
Elongation At Break /% | ASTM D412 | 370 | 282 | 263 | 310 |
Tear Strength/KN/m | ASTM D624-B | 17 | 17 | 18 | 17 |
*Heat Resistance | Hardness change /shore A | +4 | +2 | +2 | +2 |
Tensile strength change, % | -24 | -25 | -23 | -26 | |
Elongation at break change, % | -19 | -10 | -14 | -12 | |
Fuel C Volume Change/% 23℃/72h | ASTM D471 | +23 | +23 | +21 | +21 |
Peel Strength/N/mm, with Methyl vinyl silicone rubber | 2.0 | 2.0 | 2.2 | 2.0 | |
Curing Condition | Add 0.8 parts of bis-di-quaternary, one-stage vulcanisation 120℃×15min, two-stage vulcanisation: 200℃×4h | ||||
Superior Resistance to Harsh Environments: FV9500 fluorosilicone rubber excels in environments with extreme temperatures and exposure to aggressive chemicals. It provides excellent resistance to fuels, oils, and a wide range of chemicals, making it ideal for demanding industrial applications.
Wide Temperature Range: This material offers a broad operating temperature range, from as low as -60°C to as high as 200°C. This makes it highly suitable for applications in automotive, aerospace, and manufacturing industries, where temperature fluctuations are common.
Excellent Compression Set Resistance: FV9500 demonstrates outstanding resistance to compression set, ensuring prolonged performance and sealing effectiveness under sustained pressure, even in high-stress conditions.
Enhanced Durability: The fluorosilicone composition enhances durability against aging, ozone, and UV exposure, ensuring long-term reliability and performance, even under harsh environmental conditions.
Superior Electrical Insulation: It provides excellent electrical insulation properties, making it ideal for use in electronic components and sealing applications where electrical resistance is crucial.
Versatility in Application: The material can be used across various industries, including automotive, aerospace, oil and gas, and electronics, due to its combination of mechanical strength and chemical resistance.
Good Flexibility and Tear Resistance: Fluorosilicone rubber FV9500 offers flexibility even at low temperatures, combined with excellent tear and abrasion resistance, ensuring reliable performance in dynamic and high-wear conditions.
Food-Grade Options Available: Depending on your requirements, fluorosilicone rubber variants can be formulated to meet food-grade standards, providing a safe solution for applications in food processing and pharmaceutical industries.