FVL-7435 Liquid Fluorosilicone

ʻO FVL-7435 Liquid Fluorosilicone Rubber he kūpaʻa maikaʻi loa ia i ke kiʻekiʻe a me ka haʻahaʻa haʻahaʻa, ka pale ʻaila a me ka insulation uila, a hiki ke ho'ōla ʻia i ka lumi wela.
  • FVL-7435

  • Herchy

Loaʻa:
Nui:

Hana Huahana

Nā mea

Nā ʻano hoʻāʻo

NFS-L-7435

Ka helehelena A

ʻike maka

melemele

Nānā B

ʻike maka

melemele

Viscosity / Pa.s A

(ka ʻoki ʻoki 10 s -1 )

Q/371002WXH028-2016

350

Viscosity / Pa.s B

(ka ʻoki ʻoki 10 s -1 )

Q/371002WXH028-2016

300

25℃×48h

Kaumaha kikoʻī/g/cm3

ASTM D792

1.42

ʻOoleʻa/PaʻaA

ASTM D2240

35

Ikaika U'i/MPa

ASTM D412

8.1

Elongation ma ka hoomaha /%

ASTM D412

320

Ka Haehae Kaha/KN/m

ASTM D624-B

14.5

ʻO ke kūpaʻa /%

ASTM D1054

36

Hoʻonohonoho hoʻoemi/%(177℃×22h)

ASTM D395

21

Huina C

Hoʻololi Volume /%

(25℃×72h)

ASTM D471

24.0

Hoʻohana:

NFS-L-7435 wai fluorosilicone rubber i hoʻopaʻa ʻia i ʻelua mau mea. I ka hoʻohana ʻana, nā ʻāpana A, B e like me ka ratio nui o ka hui ʻana o 1: 1 a me ka hoʻomaʻamaʻa defoaming, ke ana wela o ka lumi (25 ℃ ± 5 ℃) i waiho ʻia i 48h hiki ke hoʻōla loa.

Hoʻopili:

Hoʻopili ʻia i loko o ka pahu plastik, 20kg no kēlā me kēia ʻāpana A/B.

Ka wā mālama:

Mālama ʻia i loko o kahi ʻāina maloʻo a maloʻo, ʻaʻole i wehe ʻia i ka wā e mālama ai i ka pahu pahu kumu no ʻumikūmālua mahina.

Nā mea e mālama ai:

E hōʻalo i ka hoʻopili ʻana me nā pūhui i loaʻa i ka nitrogen, sulfur, phosphorus a me nā metala kaumaha, hiki ke hoʻomākeʻe ka huahana i ka vulcanise me ka ʻole a i ʻole ka vulcanise.

Mua: 
Aʻe: 

NUI WIWIKI

KO MAKOU HANA

IKE HOPE

Hoʻohui: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Kuleana kope     2023 Shanghai Herchy Rubber Co., Ltd. Palapala kahua |   Kulekele pilikino | Kākoʻo Na Leadong.